2020 BURNDY Master Catalog
Exothermic Grounding
Making a BURNDYWeld ® Connection
Making a BURNDYWeld ® Connection
Step 1 Position cleaned conductors in mold after make sure mold is dry, by pre-heating or making a test joint.
Step 2 Place metal disc in bottom of mold crucible.
Step 3 Dump powder into crucible, being careful not to loosen all the starting powder.
Step 4 Close lid and place a small amount of starting powder in the ignition pocket.
Step 6 Wait 15 seconds, then remove weld and clean mold before making next connection.
Step 5 Ignite the starting powder with the Flint Ignitor.
1-800-465-7051 (Canada) 1-603-647-5299 (International)